  • DEUTSCH, seite 43
Oxidations
Cause
Insufficient gas protection.
Solution
Adjust the gas flow.
Check that the diffuser and the gas nozzle of the
torch are in good condition.
Porosity
Cause
Grease, varnish, rust or dirt on the workpieces to
be welded.
Solution
Clean the workpieces carefully before welding.
Cause
Grease, varnish, rust or dirt on the filler material.
Solution
Always use quality materials and products.
Keep the filler metal always in perfect condition.
Cause
Humidity in the filler metal.
Solution
Always use quality materials and products.
Keep the filler metal always in perfect condition.
Cause
Incorrect arc length.
Solution
Decrease the distance between the electrode and
the piece.
Cause
Humidity in the welding gas.
Solution
Always use quality materials and products.
Ensure the gas supply system is always in perfect
condition.
Cause
Insufficient shielding gas.
Solution
Adjust the gas flow.
Check that the diffuser and the gas nozzle of the
torch are in good condition.
Cause
The weld pool solidifies too quickly.
Solution
Decrease the travel speed while welding.
Pre-heat the workpieces to be welded.
Increase the welding current.
Hot cracks
Cause
Incorrect welding parameters.
Solution
Decrease the welding voltage.
Use a smaller diameter electrode.
Cause
Grease, varnish, rust or dirt on the workpieces to
be welded.
Solution
Clean the workpieces carefully before welding.
Cause
Grease, varnish, rust or dirt on the filler metal.
Solution
Always use quality materials and products.
Keep the filler metal always in perfect condition.
Cause
Incorrect welding mode.
Solution
Carry out the correct sequence of operations for
the type of joint to be welded.
Cause
Pieces to be welded have different characteristics.
Solution
Carry out buttering before welding.
Cold cracks
Cause
Humidity in the filler metal.
Solution
Always use quality materials and products.
Keep the filler metal always in perfect condition.
Cause
Particular geometry of the joint to be welded.
Solution
Pre-heat the pieces to be welded.
Carry out post-heating.
Carry out the correct sequence of operations for
the type of joint to be welded.
For any doubts and/or problems do not hesitate to contact