Polymerization
P lace the clamped flask in a cold water bath and heat slowly up to 100 °C / 212 °F.
Polymerization time: Boil for 1 h @ 100 °C / 212 °F.
Then allow the flask to cool down slowly. Do not quench with cold water.
Polymerization in microwave device
P olymerization takes place in suitable commercially available microwave flasks (plastic, suitable for pressing)
at 850 watts within 10 minutes. Microwave-compatible dental plasters must be used for investing. Investing
and polymerization must be carried out within 8 hours. Units without a rotary plate may necessitate gradual
polymerization on all sides by turning of the flask. De-flask after self-cooling down to room temperature.
Trimming of the denture
T rim the acrylic as usual. PERMALINER can be machined with milling cutters or grinding sleeves (15,000 –
20,000 RPM) without heat build-up. Rough spots can be removed with polishing discs.
Polishing of the acrylic
P re-polish and mirror-polish acrylic in the conventional way. PERMALINER cannot be mirror-polished.
Lustrol gloss varnish is recommended as an alternative. The dosage is 1:1. Before application, the base and
functional borders must be clean and dry. Apply Lustrol using a brush and let it dry for about 10–15 minutes.