Check the tightness of the screw connections with foaming agents (e.g. leak detection spray
ROTEST, Art.-No. 65000).
Close the cartridge valves in case of an accident, or after use.
Depressurize the hoses after completing work by opening the valves on the handle while the
pressure reducers are closed, then close the valves on the handle again.
Do not use the unit in a horizontal position.
Keep the unit free from oil and grease. Oils and greases of all kinds can self-ignite explosively in
pure oxygen.
1.2

Intended use

Congratulations on your purchase of a ROTHENBERGER brand product. With the ALLGAS
Mobile Pro, you have purchased a quality product. This portable, universal autogenous welding
equipment is ideal for brazing and welding up to a material thickness of 5.0 mm.
2

Technical data / range of application

Flame temperature ................................
Working temperature ................................
Choose the appropriate solders and solder pastes based on the working temperature
Gas type ................................
Gas pressure ................................
Working range ................................
Welding tips
Tip size
(material thickness in mm)
1
2
3
4
5
3

Function of the Unit

Welding with high-power welding tips:
Basically, the welding flame should burn neutral (the mixing ratio of gases is balanced), and its
size should be adjusted to the material thickness, the bead shape, the welding position and the
thermal conductivity of the material.
For welding steel with larger thickness both valves should be wide open and for welding of steel
sheets with low material thickness the valves should be turned back slightly.
Preheat material and welding rod. Once the metal begins to melt on both sides of the seam, add
the welding rod. Look for a uniform heating of the weld. Lead the burner in semi-circular move-
ments around the welding rod.
Brazing:
Deburr the joint surface and make it metallic bright (free of dirt and oxide), e.g. with the metal-
free ROVLIES cleaning pad (Art.-No. 45268). Preheat solder joint. Add the tip of the solder rod
on top of the solder joint, melt a drop of solder and spread it with constant movement of the
flame.
10
more than 3.100 °C
more than 1.300 °C
MAPP, oxygen
disposable MAPP-gas cartridge: 9 bar, with pressure reducer: max. 2
bar
disposable oxygen cartridge: 110 bar, with pressure reducer: max. 4 bar
0,2-5,0 mm material thickness
Working range
0,2 – 1
1 – 2
2 – 3
3 – 4
4 – 5